Technical Data
ASC2250® LDX Welding and Machining
GENERAL WELDING INFORMATION
Gas Tungsten arc TIG | (GTAW) |
Shielded Metal arc | (SMAW) |
Gas Metal arc | (GMAW) |
Flux-cored arc | (FCW) |
Submerged arc | (SAW) |
Plasma arc | (PAW) |
Resists the negative effects of localized corrosion in welding, at the heat affected zone. Request detailed welding information
Welding Tips
No pre-heat required. Cool between passes (below 300°F). Filler metal suggested but not required. Post weld anneal not required. If post-weld annealing is accomplished, follow with a rapid water quench to prohibit re-forming of the intermetallic phase.
When using GTAW or PAW, consider the adding of nitrogen in the shielding/purging gas to ensure optimum pitting resistance. Recommended Fillers: LDX2101 from Avesta Welding or 2209. Request detailed welding data.